@Article{, title={Influence of Doping on K2SO4 Crystal Properties اثر التطعيم في خصائص بلورة كبريتات البوتاسيوم K2SO4}, author={Tariq A.Al- Dahair طارق عبد الرضا الظاھر and Maryam E.Al-Mahdawy مريم عيسى المھداوي}, journal={Ibn Al-Haitham Journal For Pure and Applied Sciences مجلة ابن الهيثم للعلوم الصرفة والتطبيقية}, volume={28}, number={1}, pages={11-23}, year={2015}, abstract={Single crystals of pure and Cu+2,Fe+2 doped potassium sulfate were grown fromaqueous solutions by the slow evaporation technique at room temperature. with dimension of(11x9 x4)mm3 and ( 10x 8x 5)mm3 for crystal doping with Cu &Fe respectively. Theinfluence of doping on crystal growth and its structure revealed a change in their latticeparameters(a=7.479 Å ,b=10.079 Å ,c=5.772 Å)for pure and doping (a=9.687 Å, b=14.926 Å,c= 9.125 Å) & (a=9.638 Å , b= 8.045 Å ,c=3.271 Å) for Cu & Fe respectively. Structureanalysis of the grown crystals were obtained by X-Ray powder diffraction measurements. Thediffraction patterns were analyzed by the Rietveld refinement method. Rietveld refinementplots for showing the experimental (red circles)calculated (black line) and difference profiles(blue line); green tick marks indicate reflection positions XRD measurements show the crystalsystem of orthorhombic.

نماء بلورات أحادية لكبريتات البوتاسيوم النقية والمشوبة ب Cu+2 وFe+2 من المحلول المائي بوساطة تقنية التبخر البطيء في درجة حرارة الغرفة. وبأبعاد ( 11x9x 4)10x 8x 5 ) mm3(mm3 للبلورات المشوبة بCu & Feعلى التوالي.ودراسة اثر التطعيم في النماء البلوري والخصائص التركيبية , إذ تغيرت أبعاد خلية الوحدة لكبريتات البوتاسيوم المطعمة بالنحاس والحديد. (a=7.479 Å ,b=10.079 Å ,c=5.772 Å)للنقية والمشوبة, (a=9.687 Å, b=14.926 Å ,c= 9.125. (a=9.638 Å , b= 8.045 Å ,c=3.271 Å) تم الحصول على تحليل بنية البلورات بوساطة مقياس حيود الأشعة السينية للمسحوق و استخدام تصفية ريتفيلد. أظهرت قياسات XRDإن التركيب البلوري لهذه البلورات هومعيني متعامد المحاور(orthorhombic).} }