TY - JOUR ID - TI - The Effect of The Electrochemical Deposition Potential Variation on The Coating of Hydroxyatite on Commertialy pure Titanium (CpTi) and Ti-6Al-4V Alloy تأثيرتغيير فرق الجهد للترسيب الكهروكيميائي للهايدروكسيأبتايت في التيتانيوم النقي تجارياً وسبيكة Ti-6Al-4V AU - Aqeel F. Hasan عقيل فليح حسن AU - Jamal F. Hammody جمال فاضل حمودي AU - Shaymaa H. Aneed شيماء هاشم عنيد PY - 2015 VL - 12 IS - 4 SP - 684 EP - 690 JO - Baghdad Science Journal مجلة بغداد للعلوم SN - 20788665 24117986 AB - In this research we investigated the corrosion behavior of the commertialy pure titanium and Ti-6Al-4V alloy that coated with hydroxyapatite by electrochemical deposition with applied voltage (6,9,12) Volt from aqueous solution containing Ca(NO3)2.H2O =7.0 gm/l , (NH4)2HPO4 =3.5 gm/l , Na(NO3)2 = 8.5 gm/l in order to improve the bonding strength of hydroxyapetite and medical metals and alloys and increasing the biocompatibility. The coating layer morphology was investigated by XRD, Optical microscope , and SEM tests, the corrosio tests was made by use senthesys simulated body fluid (SBF) , and we found that the propreate voltage for coatint on Ti was 9 Volt and for Ti-6Al-4Vwas12Volt.

في هذا البحث تمت دراسة السلوك التاكلي للتيتانيوم النقي تجارياً ولسبيكة Ti-6Al-4V المطليين بالهايدروكسيأبتايت بطريقة الترسيب الكهروكيميائي بعد تسليط فرق جهد (12,9,6) فولت وباستعمال المحلول المائي الحاوي على المركبات Ca(NO3)2.H2O 7.0 gm/L,(NH4)2HPO4 3.5 gm/L ,Na(NO3)2 8.5 gm/lلإجل تحسين قوة الترابط بين الهايدروكسيأبتايت والمعادن والسبائك الطبية وزيادة التوافقية الإحيائية. وتمت دراسة طبيعة طبقة الطلاء بإجراء فحوصات حيود الأشعة السينية وفحص المجهر البصري وفحص المجهر الألكتروني الماسح SEM , واجراء فحوصات التاكل عليها باستعمال محلول مشابه لمحاليل الجسم محضر مختبرياً (SBF), وتبين بأن أفضل فرق جهد لطلاء التيتانيوم كان 9 فولت أما لسبيكة Ti-6Al-4V فكان 12 فولت . ER -