@Article{, title={The Effect of Annealing on The Structural and Optical Properties of CdO Thin Films by Chemical Bath Deposition Technique تأثير التلدين على الخصائص التركيبية والبصرية لأغشية CdO الرقيقة المحضرة بتقنية الترسيب بالحمام الكيميائي (CBD)}, author={Hani H. Ahmed هاني هادي احمد and Rafea A.Munef رافع عبدالله منيف and Faris S. Atallah فارس صالح عطالله}, journal={Academic Science Journal مجلة العلوم الاكاديمية}, volume={12}, number={2}, pages={20-31}, year={2016}, abstract={In this work CdO films were prepared by chemical bath deposition technique(CBD) where the cadmium nitrat salt was used as a source of cadmium ions(Cd+2) , the effect of the annealing at (373,473.573,673) K for 60 min on the structural and optical properties is described. The XRD studies revealed the annealing temperature chosen is 673K which conversion of cadmium hydroxide film to cadmium oxide film we get to cubic structure with preferential orientation along the (111) crystal plane. The optical properties study by transmission spectra where found the CdO films have highly transmittance in visible region of spectrum and reach to more than 72 %. The CdO films have wide band gap of 2. 38 to 2.55 eV.

في هذا البحث تم تحضير غشاء CdO بتقنية ترسيب بالحمام الكيميائي (CBD) على أرضيات زجاجية ،حيث استخدم ملح نترات الكادميوم Cd(NO3)2.4H2O) كمصدر لايونات الكادميوم (2+Cd) تم دراسة تأثير درجة حرارة التلدين عند مدى درجات الحرارة K (373,473,573,673) ولمدة 60min على الخصائص التركيبية والبصرية للغشاء المحضر. نتائج حيود الأشعة السينية (XRD) بينت إن أفضل درجة حرارة تلدين هي 573K التي يمكن الحصول فيىا على الطور المكعب (Cubic) لغشاء CdO بافضل اتجاهية بلورية عند المستوي (111). الخصائص البصرية بينت إن الغشاء المرسب يمتلك نفاذية عالية ضمن المدى المرئي من الطيف وتصل الى أكثر من 72% وفجوة طاقة عريضة تمتد من 2.38eV إلى2.55eV.} }