TY - JOUR ID - TI - Study the Effect of Electrodeposition Parameters on Ni/SiC Composite Coating AU - Fatima N. Jaseem AU - Mofeed A.L. Jaleel PY - 2017 VL - 20 IS - 4 SP - 1005 EP - 1011 JO - Al-Nahrain Journal for Engineering Sciences مجلة النهرين للعلوم الهندسية SN - 25219154 25219162 AB - In this research, we successfully obtained Ni/SiC micro-composite coatings with various contents of SiC particles of particle size(10 µm), by using electrodeposition method from nickel watts bath in which the SiC particles suspend. The effects of the current density, temperature, and particle loading(PL) of SiC particles in the electrolyte on the morphology, texture, and vol% of SiC in deposit were investigated. The morphological and structural analysis show uniform distribution of SiC particles within the composite coatings. It was found that the depositing conditions affect the microstructure of deposited nickel and the SiC vol% in deposit. Furthermore, the vol% of SiC increases in deposit by increasing the particle loading(PL) in the bath, while decreased by increasing the current density. Also the higher values of SiC vol% were obtained at temperature (50°C).

في هذا البحث تم تحضير الطلاء المتراكبة Ni/SiC بنسب مختلفة من دقائق كاربيد السيليكون داخل حمام الطلاء ذات الحجم الحبيبي (10 µm) بأستخدام طريقة الترسيب الكهربائي وباستخدام حمام واتس الذي تتشتت داخله دقائق SiC. حيث تمت دراسة تأثير كل من كثافة التيار, درجة حرارة حمام الطلاء, وتركيز الدقائق داخل حمام الطلاء على كل من مورفولوجيا السطح, التركيب, والنسبة الحجمية للدقائق داخل الطلاء. ان التحليل التركيبي للطلاء اظهر التوزيع المتجانس للدقائق داخل الطلاء. ووجد بأن شروط الترسيب لها تأثير على التركيب المايكروي لطلاء المتراكبات وكذلك على النسبة الحجمية للدقائق داخل الطلاء. علاوة على ذلك, فأن النسبة الحجمية للدقائق داخل الطلاء تزداد بزيادة تركيز الدقائق في حمام الطلاء, بينما تقل بزيادة كثافة تيار الترسيب. كما ان اعلى قيمة لااندماج الدقائق كانت عند درجة حرارة 50 OC. ER -