@Article{, title={Structural Behavior of Composite Castellated Steel Concrete Beams Subjected to Impact Load}, author={Shereen Q. Abdulridha and Haitham H. Muteb and Sarmad Sh. Abdulqader}, journal={Journal of University of Babylon مجلة جامعة بابل}, volume={26}, number={8}, pages={1-12}, year={2018}, abstract={The structural behavior of composite castellated steel concrete beams subjected to impact load presented in this study. In which fabrication of composite castellated steel self-compacting concrete beams which connected to self-compacting concrete by means of stud shear connectors. Four composite castellated beams were performed with different degrees of castellation, they were 0%, 25%, 33.8% and 50%. These specimens were subjected to an impact load produced from free falling of steel ball. The experiments required fabrication of special rig which connected with different sensors and programmed by Lab VIEW 2016 program. Different parameters were recorded and discussed which involved force-time history and displacement history for the tested beams. It is founded that the increase of the degrees of castellation for the adoptedspecimens will increase the maximum impact load by about 16.13%, compared with non-castellated composite specimen. The amplitudes of vibration represented by displacement have decreased with the increasing of degrees of castellation by about 3.51%, 14.04% and 20.18% for the degrees of castellation 25%, 33.8%, and 50% respectively.

تشملالدراسةالحالية تصنيعالعتباتالمعرشةالتيترتبطبالخرسانةذاتيةالانصهاربواسطةوصلاتربطلدراسةسلوكهاتحتتأثيرالاحمال الصدمية. تمتنفيذأربعةعتباتمركبةومعرشةبدرجاتمختلفةمنالتعريش هي 0% و25٪ و33,8٪ و50٪. تعرضتهذهالعيناتلحملالصدمةالناتجةعنالسقوطالحرللكرةالفولاذية.تطلب اجراء الفحوصات المختبرية تصنيع جهاز خاص تم توصيله بمتحسسات مختلفة وتمت عملية برمجتها باستخدام برنامج Lab VIEW 2016.تمتسجيلومناقشةمعاملاتمختلفةوالتيتضمنتمخطط القوةمع الزمن ومخطط الانحراف مع الزمن للحزمالتيتماختبارها.زادالحدالأقصىللحمل الصدميمعزيادةدرجاتالتعريشالتيتمتبنيهابنسبة 16,13٪ تقريبًا. وقدانخفضتسعةالاهتزازالمتمثلةفيالانحرافمعزيادةدرجاتالتعريشبنسبة 3,51٪ و14,04٪ و20,18٪ لدرجاتالتعريش 25% و33,8% و50% على التوالي.} }