TY - JOUR ID - TI - Tensile Strength Determination of heat Treated Austenitic Stainless Steel AISI 316L Using (ABI) Method ايجاد مقاومة الشد القصوي للصلب المقاوم للصدأ اللاوستنايتي AISI 316L المعامل حراريا وذلك باستخدام تقنية (ABI) AU - Ramadhan H. Gardi رمضان حسين الجردي PY - 2012 VL - 20 IS - 2 SP - 98 EP - 105 JO - AL-Rafidain Engineering Journal (AREJ) مجلة هندسة الرافدين SN - 18130526 22201270 AB - AbstractIn this study, austenitic stainless steel AISI 316L has been selected to investigate the effect of aging time and temperature on tensile strength using (ABI) technique. Heat treatment consisted of aging at temperature of 400 oC, 600 oC and 800 oC and socking time for 0.5, 1.5, 10, 24 and 72 hrs.For microstructure examination, an optical microscope were used. The results showed that with increasing the aging time at 400 oC and 600 oC the tensile strength will increase but this approach inverted at 800 oC. These results could be attributed to some metallurgical transformation that occurs during heat treatment like changing in grain size, carbide and nitride precipitation along the grain boundaries, and secondary austenite.KEY WORDS: Tensile strength, 316L, austenitic stainless steel, ABI, heat treatment

الخلاصةفي هذه الدراسة استخدمت سبيكة الصلب المقاوم للصدا الآستنايتى AISI 316L لتحديد تاثير التغيرات الميتالورجية التى تحصل نتيجة المعاملات الحرارية علي مقاومة الشد القصوي وذلك باستخدام تقنية (ABI) (Automated Ball Indentation). المعاملة الحرارية تتكون من التعتيق في ثلاث درجات الحرارية المختلفة (400 oC,600 oC,800 oC )و لخمسة فترات زمنية مختلفة (0.5,1.5,10,24,72)ساعة لكل درجة.اضهرت النتائج بان زيادة زمن التعتيق من oC 400 و 600 oC ان مقاومة القصوي تزداد و لكن المادة تتصرف عكس ذلك في درجة الحرارة 800 oCوان اسباب هدة النتائج تعود بشكل اساسي الي التغيرات الميتالورجية في الصلب اللاوستنايتي ومن بين هدة التغيرات التحولات الطورية,تغير حجم البلورات ،ترسيب كاربيدات ونتريدات علي حدود البلورات،.......الخالكلمات الدالة:مقاومة الشد،الصلب الاوستنايتيكى،ABI،المعاملة الحرارية ER -