@Article{, title={A STUDY ON PLASTIC CONTAINERS TO REDUCE THEIR EFFECT ON THE ENVIRONMENT دراسة للتخلص من النفايات البلاستيكية لتقليل أضرارها البيئية}, author={Hameed K. Ali Al-Dulaimy حميد خالد علي الدليمي}, journal={IRAQI JOURNAL OF DESERT STUDIES المجلة العراقية لدراسات الصحراء}, volume={2}, number={1}, pages={53-60}, year={2010}, abstract={ABSTRACT: This study had been carried out on the photo degradation of polystyrene films accelerated by new photosensers derived from Nickel (II) and Schiff bases; the complex was identified by its I.R spectrum, melting point and other physical properties. It was added on the polystyrene films by the following percentages (0.025%, 0.03%, 0.05%, 0.07% and 0.1%) respectively. Then, it was irradiated by accelerated U.V light (350 nm) at 40 Co for different time intervals, and the degree of degradation was estimated by calculating both (IOH) and (ICO). The obtained results are in a good agreement with those of polymers surfaces responded for degradation agents; yet reported. The best degradation results were given by the (0.05%) system while (0.1%) and gave the lowest result as indicated by both I.R and U.V Spectra.

المستخلص:تمت في هذا البحث دراسة التجزئة الضوئية لرقائق متعدد الستايرين والمعجل بمحفز ضوئي جديد من أحد معقدات النيكل الثنائي والمشتق من قواعد شف . شخص المعقد بمطيافية I.R و UV ودرجة الانصهار والخواص الفيزيائية الأخرى .تم إضافة المعقد بنسب وزنية (0.025% , 0.03%, 0.05% , 0.07% , 0.1% ) على رقائق متعدد الستايرين . وأجري التشعيع المسرع بأشعة U.V بطول موجي 356 نانومتر ولازمان مختلفة وبدرجة حرارة 40 م .وتم احتساب مقدار التفكك بمتابعة قيم (IOH) و (Ico) , وجائت نتائج هذه الدراسة متطابقة مع ما أظهره سطح البوليمر من استجابة لعوامل التفكك . وأعطت نسبة الإضافة من المعقد( 0.05%) الى الرقائق أعلى نسبة للتفكك , بينما أعطت نسبة الإضافة (0.1 % ) أوطأ قيمة للتفكك , والذي جرى متابعته باستخدام مطيافية U.V و I.R، وكان متفقا مع الأدبيات .} }