TY - JOUR ID - TI - Types of the Fiber Glass-Mat on Fatigue Characteristic of Composite Materials at Constant Fiber Volume Fraction: Experimental Determination تأثير نوع حصيرة الا لياف الزجاجية على سلوك الكلال للمواد المتراكبة عند نسبة حجميه ثابتة للالياف الزجاجية AU - Hussain J. Al-Alkawi حسين جاسم العلكاوي AU - Dhafir S. Al-Fattal ظافر صادق الفتال AU - Abdul-Jabar H. Ali عبد الجبار حسين PY - 2012 VL - 8 IS - 3 SP - 1 EP - 12 JO - Al-Khwarizmi Engineering Journal مجلة الخوارزمي الهندسية SN - 18181171 23120789 AB - The aim of this work is to study the influence of the type of fiber glass –mat on fatigue behavior of composite material which is manufactured from polyester and E-glass (woven roving, chopped strand mat (CSM)) as a laminate with a constant fiber volume fraction (VF) of 33%. The results showed that the laminates reinforced with E-glass (woven roving) [0/90, ±45.0/90] and [0/90, CSM, 0/90] have lower fatigue strength than the laminates reinforced with E-glass [0/90]3,[CSM]3 and [CSM, 0/90, CSM] although they had different tensile strength; the best laminate was [0/90]3 .

يهدف البحث الحالي الى دراسة تأثير نوع طبقات اللالياف الزجاجية على سلوك الكلال للمواد المتراكبه المصنعه من البولستر وبنسبه حجميه ثابتة للألياف الزجاجية مقدارها 33%. أظهرت نتائج البحث ان المواد المصنعه من ] [0/90, CSM, 0/90], [0/90,±45, 0/90 تمتلك أدنى حد للكلال عند 107 من تلك للمواد المصنعه من[0/90]3 و,[CSM, 0/90, CSM] [CSM]3 على الرغم من انها تمتلك اجهاد شد اقصى مختلف وان أفضل الطبقات هي[0/90]3. ER -