research centers


Search results: Found 12

Listing 1 - 10 of 12 << page
of 2
>>
Sort by

Article
Characteristics and Properties of Epoxy/Polysulfide Blend Matrix Reinforced by Short Carbon and Glass Fibers
بعض الخصائص الميكانيكية لمتراكبة خليط الايبوكسي-بولي سلفايد المدعم بألياف الكربون والزجاج القصيرة

Authors: Ibtihal A. Mahmood ابتهال عبد الرزاق محمود --- Mustafa Ziyara Shamukh مصطفى زيارة شامخ
Journal: AL-NAHRAIN JOURNAL FOR ENGINEERING SCIENCES مجلة النهرين للعلوم الهندسية ISSN: 25219154 / eISSN 25219162 Year: 2017 Volume: 20 Issue: 1 Pages: 80-87
Publisher: Al-Nahrain University جامعة النهرين

Loading...
Loading...
Abstract

In this research, binary blends have been prepared from epoxy resin (EP) and different weight percentages of polysulfide rubber (PSR) (0%, 2.5%, 5%, 7.5 and 10%), and then compression, impact, and hardness tests were evaluated. The experimental results showed that the addition of polysulfide rubber in the epoxy resin decreased the compressive strength, Young's modulus, and hardness, while increased the impact resistance. It was found that the weight percentage 5% of polysulfide was the best percentage, which gives the best mechanical properties for the blend matrix. The advantage of this blend matrix is that, it mediates between the brittle properties of epoxy and the flexible properties of a blend matrix with the highest percentage of PSR. Short fibers (Carbon & Glass) with different volume percentage (2.5%, 5%, 7.5%, and 10%), were used to reinforce the best blend matrix obtained separately and randomly, and then the same mechanical tests conducted on these composites. The experimental results showed that the addition of fibers increased the compressive strength, Young's modulus, impact resistance and hardness. It was also observed that the composites materials reinforced with carbon fibers have significantly higher mechanical properties values than the composites materials reinforced with glass fibers.

في هذا البحث, تم تحضير خلطات ثنائية من راتينج الايبوكسي مع عدة نسب وزنية مختلفة من مطاط البولي سلفايد (0% , 2.5% , 5% , 7.5% , 10%), ومن ثم تم اجراء عليها اختبار الانضغاط, اختبار الصدمة, واختبار الصلادة. النتائج التي تم الحصول عليها أظهرت بأن الزيادة في نسبة البولي سلفايد تؤدي الى نقصان في قيمة الاجهاد الأقصى, معامل يونج, والصلادة وبينما تؤدي الى زيادة قيمة مقاومة الصدمة. افضل النتائج الميكانيكية التي تم الحصول عليها عند خلط 5% من مطاط البولي سلفايد مع الايبوكسي. تم استخدام الياف قصيرة من الكربون والزجاج مع عدة نسب حجمية مختلفة (2.5%, 5%, 7.5%, 10%) لتدعيم الخليط الأمثل الذي تم الحصول عليه بشكل منفصل وعشوائي, ومن ثم تم اجراء نفس الاختبارات السابقة عليها. النتائج المستحصلة أظهرت بأن الزيادة في نسبة الالياف تؤدي الى زيادة في قيمة الاجهاد الأقصى, معامل يونج, مقاومة الصدمة, والصلادة. وقد لوحظ ايضاً بأن المواد المتراكبة المدعمة بواسطة الياف الكربون أعطت قيم عالية من الخواص الميكانيكية مقارنة بالمواد المتراكبة المدعمة بواسطة الياف الزج.


Article
EXPERIMENTAL STUDY OF SOUND ABSORPTION PROPERTIES OF REINFORCEDPOLYSTER BY SOME NATURAL MATERIALS
دراسة عملية لخواص امتصاص الصوت للبولستر المقوى ببعض المواد الطبيعية

Author: Dr. Muna S. Kassim د منى صباح قاسم
Journal: Iraqi journal of mechanical and material engineering المجلة العراقية للهندسة الميكانيكية وهندسة المواد ISSN: 20761819 Year: 2017 Volume: 17 Issue: 4 Pages: 798-812
Publisher: Babylon University جامعة بابل

Loading...
Loading...
Abstract

Sound absorption in living, traveling and working environment constitutes one of the major requirements for human comfort today. Sound insulation requirements in automobiles, in manufacturing environments, and in equipments, generating higher sound pressure, strives the need to develop more efficient and economical ways of producing absorption materials. Traditionally, economics of recent research has enforced the research to focus on waste materials. The aim of this study is to use waste materials (particles of egg shell, palm leaf, jute, wood dust, chicken feather) for producing reinforced and polyester resien composite structures with 17% weight fraction. Two natural material composite plate shapes (flat and corrugated) with the same area is manufactured, where the echoic chamber is built and insulated with cork and sponge for different inside wall shape (flat, concave and pyramids) . The study concluded that the jute woven and saw dust composite exhibited a greater ability to absorb normal incidence sound waves than the composites with chicken feather, particles of egg shell, and palm leaf fiber for different shape cork and sponge insider insulator. The analysis of sound transmission loss revealed that the particles of egg shell and saw dust still obeyed the mass law of transmission loss. The composite surface layer of particles of egg shell and saw dust possessed a higher fabric density and therefore showed a better sound insulation than the composites with jute woven, chicken feathers, and palm leaf.

يعتبر امتصاص الصوت من اهم متطلبات راحة الانسان في محيط المعيشة والتنقل والعمل. ان الحاجة الى العزل الصوتي في وسائط النقل واجواء المصانع وفي المعدات التي يكون فيها ارتفاع ضغط صوتي حاجة ماسة لتطوير مواد ماصة للصوت تكون ذات كفاءة اعلى واقتصادية اكثر. يركز البحث الحالي من الناحية التجارية والاقتصادية على المواد المهملة . يتناول البحث الحالي دراسة العزل الصوتي للمواد المركبة المصنعة من : قشور البيض ، ليف النخيل، الجوت، نشارة الخشب وريش الدجاج) مع البوليستر لنسبة وزنية تساوي 17%. لقد تم دراسة شكلين من الصفائح هما: الصفيحة المستوية والصفيحة المتعرجة. كما تم تصنيع غرفة العزل الصوتي وتم وضع الاسفنج والفلين كمواد عازلة من الداخل وتغيير شكل هذه العوازل (مستوي ومحدب وهرمي ) .لقد استنتجت الدراسة ان المواد المركبة من حصيرة الجوت ونشارة الخشب لها قابلية عالية لامتصاص الضوضاء بالمقارنة مع ريش الطيور وحبيبات قشور البيض وليف النخيل لمختلف اشكال العوازل الداخلية (الفلين، الاسفنج) للغرفة المستخدمة. ان تحليل خسائر انتقال الصوت اظهرت ان المركبات المكونة من نشارة الخشب وحبيبات قشور البيض تقع ضمن قانون الكتلة لخسارة الانتقال حيث ان مركبات هاتين المادتين لها كثافة بناء عالية لهذا فهي عوازل صوتية افضل من مركبات حصيرة الجوت و ريش الطيور وليف النخيل .


Article
STUDY THE EFFECT OF THE PARTICLE SIZE ON MECHANICAL PROPERTIES OF PARTICULATE NATURAL COMPOSITE MATERIALS

Author: Israa Faisal Qhazi
Journal: Al-Qadisiyah Journal for Engineering Sciences مجلة القادسية للعلوم الهندسية ISSN: 19984456 Year: 2017 Volume: 10 Issue: 2 Pages: 120-132
Publisher: Al-Qadisiyah University جامعة القادسية

Loading...
Loading...
Abstract

This research studied the mechanical properties of particulates composite materials made from natural fillers (eggshell and sawdust) reinforced epoxy resin. The composite specimens were prepared by hand lay-up technique with one volume fraction Vf, and different particle size of fillers.Modulus of elasticity, tensile strength, percentage of elongation and hardness were measured for each type of composite. The tensile tests results had shown an incremental increase with size of particles decreasing also hardness results had shown an incremental increase with smaller particle size.This work institutes a good substitution for synthetics fillers avoiding their highly cost and their toxicity, at the same time reducing of the environmental pollution.


Article
Studying the Effect of Mixture of Pomegranate Peel and Licorice on the Mechanical Properties of Epoxy

Author: Najmuldeen Yousif Mahmood
Journal: AL-NAHRAIN JOURNAL FOR ENGINEERING SCIENCES مجلة النهرين للعلوم الهندسية ISSN: 25219154 / eISSN 25219162 Year: 2017 Volume: 20 Issue: 4 Pages: 871-875
Publisher: Al-Nahrain University جامعة النهرين

Loading...
Loading...
Abstract

Reinforcement process of epoxy has been widely used to improvement of mechanical properties. Therefore, this work is concerned with the reinforcement of epoxy by adding natural materials (Pomegranate peel and Licorice particles) at epoxy. Different percentages of particles (5, 10, 15 and 20%) were used. The mechanical testing were included tensile, bending, hardness and impact tests. Hardness of epoxy was increased at increasing of Pomegranate peel (PP) and Licorice (L) percentages. Impact resistance of epoxy with Pomegranate peel (PP) has reached the highest at (10%), while with Licorice (L) has reached the highest at (5%). The results of tensile strength represent that increases of tensile strength at all percentages of (L), while (PP) showed that decreases at (5%) and increases at others percentage. Bending strength of epoxy has increased as increasing of (PP) at all percentage that used, but it has increased at (5, 10 and 20%) of (L), while it has dropped at (15%).

استخدمت عملية تقوية الايبوكسي على نطاق واسع لتحسين الخواص الميكانيكية. لذلك تعلقت الدراسة بتقوية الايبوكسي بأضافة المواد المواد الطبيعية (دقائق قشور الرمان وعرق السوس) الى الايبوكسي. استخدمت نسب مختلفة من الدقائق (5, 10, 15 و 20%). الاختبارات الميكانيكية تظمنت اختبارات الشد , الانحناء , الصلادة و الصدمة. تزداد صلادة الايبوكسي بزيادة نسبة قشور الرمان وعرق السوس. وصلت مقاومة الصدمة للايبوكسي اقصى قيمة عند (10%) من قشور الرمان بينما وصلت القيمة القصوى لمقاومة الصدمة عند (5%) من عرق السوس. بينت نتنائج مقاومة الشد زيادة عند كل نسب عرق السوس بينما تتناقص عند (5%) وازدات عند باقي النسب من قشور الرمان. مقاومة الانحناء للايبوكسي تزداد بزيادة قشور الرمان عند كل النسب في حين تزداد مقاومة الانحناء عند (5 , 10 و 20%) من عرق السوس وتنخفض عند (15%).


Article
Preparation of the Jaws Damaged Parts from Composite Biopolymers Materials

Authors: Riyam A. Al-husseini --- Nehad A. Saleh --- M. H. Al-Maamori
Journal: Journal of University of Babylon مجلة جامعة بابل ISSN: 19920652 23128135 Year: 2017 Volume: 25 Issue: 2 Pages: 581-575
Publisher: Babylon University جامعة بابل

Loading...
Loading...
Abstract

Composite materials composing of fusing two materials or more are disaccorded in mechanical and physical characteristics, The studied the effect of changing in the reinforcement percentage by Hydroxyapatite Prepared nano world via the size of the nanoscale powder manufacturing manner chemical precipitation and microwave powders were two types their preparations have been from natural sources: the first type of eggshells and the other from the bones of fish in mechanical Properties which include the tensile strength, elastic modulus, elongation, hardness and tear for composite material consisting of Silicone rubber (SIR) reinforced by (µ-n-HA), after strengthening silicone rubber Protect proportions (5,10,15,20 wt%) of Article achieved results that increase the additive lead to increased hardness while tougher and modulus of elasticity decreases with added as shown in the diagrams.

المواد المتراكبة تتكون من خلط مادتين او كثر وتكون مختلفة في الخواص الميكانيكية والفيزيائية , تم دراسة تأثير اضافة هيدروكسي ابتايت كمادة مقواة محضرة بحجم نانوي مايكروي تم تصنيع المسحوق النانوي بطريقة الترسيب الكيميائي والمساحيق المايكروية كانت بنوعين تم تصنيعهما من مصادر طبيعية : النوع الاول من قشور البيض والاخر من عظام الاسماك. على الخصائص الميكانيكية التي تتضمن مقاومة الشد, معامل المرونة, الاستطالة, الصلادة والتمزق للمادة المتراكبة التي تتكون من مطاط السيليكون مدعمة بـ(مايكرو – نانو) هيدروكسي ابتايت, بعد تدعيم مطاط السيليكون بنسب تحميل (5,10,15,20 wt%) من المادة حقق النتائج ان زيادة المادة المضافة تؤدي الى زيادة الصلادة بينما اشد ومعامل المرونة تقل مع الاضافة كما موضح في المخططات.


Article
Experimental Study of the Hygrothermal Effect on Wear Behavior of Composite Materials

Authors: Fadhel Abbas. Abdulla --- Katea L. Hamid
Journal: Journal of University of Babylon مجلة جامعة بابل ISSN: 19920652 23128135 Year: 2017 Volume: 25 Issue: 4 Pages: 1373-1383
Publisher: Babylon University جامعة بابل

Loading...
Loading...
Abstract

The hygrothermal effect on the wear behavior of composite material (fiberglass and polyester resin vf=40%) was investigated experimentally in this work. The study includes manufacturing of test device (pin on disc) according to ASTM G 99. In order to study the hygrothermal effect on wear behavior of composite materials the hygrothermal chamber was manufactured. The experimental results show that the wear of glass fiber/polyester increased with increasing the load, sliding speed and sliding distance. The load and sliding distance were more effective on the wear of the composite rather than sliding speed. Also, it has been revealed that, the hygrothermal is considerable effect that, the wear rate of glass fiber/polyester without hygrothermal effect is lower than wear with hygrothermal effect. Applied load is the wear factor that has the highest physical influence on the wear of composites materials than other wear factors. Also, the wear of glass fiber/polyester without hygrothermal effect is lower than wear with hygrothermal effect.

تم دراسة تأثير الحرارة الرطبة على سلوك التأكل للمواد المركبة (الألياف الزجاجية والبوليستر الراتنج ,كسر حجمي= 40٪) تجريبيا في هذا العمل. وتشمل الدراسة تصنيع جهاز الاختبار (pin-on-disc من أجل دراسة تأثير الحرارة الرطبة على سلوك التآكل للمواد المركبة تم تصنيع غرفة الحرارة الرطبة. وأظهرت النتائج التجريبية أن تآكل الألياف الزجاجية / البوليستر يزداد مع زيادة الحمل، سرعة الانزلاق ومسافة الانزلاق. وكان الحمل ومسافة الانزلاق أكثر فعالية على تأكل المواد المركبة مقارنة من سرعة انزلاق. وقد تم الكشف عن أن للحرارة الرطبة تأثير كبير أن معدل تآكل الألياف الزجاجية / البوليستر ويكون معدل تأكل الألياف الزجاجية والبوليستر بدون تأثير الحرارة الرطبة أقل من ذلك مع تأثير الحرارة الرطبة. الحمل هو عامل التآكل الذي لديه أعلى التأثير على تاكل المواد المركبة مقارنة بعوامل التآكل الاخرى. أيضا، تآكل الألياف الزجاجية / البوليستر دون تأثير الحرارة الرطبة أقل من التآكل مع تأثير الحرارة الرطبة.


Article
Preparation and Characterization of A New Nano-scaled Material Composed of Bentonite-Polyethylenglycophthalate
تحضير و تشخيص مادة نانوية متراكبة جديدة مكونة من البنتونايت- بولي اثيلين كلايكولفثاليت

Loading...
Loading...
Abstract

In this study a new composite material have been prepared and characterized through polymerization of ethylene glycol located between the Bentonite layers with phthalic anhydride. The results showed that the polymer binds with the structure of clay through hydrogen bonding also the polymerization process led to shatter of the three-dimension crystal structure of the clay and isolating layers in the form of nano-scale two-dimensional sheets, the polymer growth around the clay isolated layers work to increase the size particles at microscopic scale.

تم في هذه الدراسة تحضير وتشخيص مادة متراكبة جديدة من خلال بلمرة الاثيلين كلايكول الموجود بين طبقات معدن البنتونايت مع مادة الفثاليك انهادرايد. بينت النتائج ان البوليمر يترابط مع هيكل الطين من خلال التاصر الهيدروجيني. ادت عملية البلمرة الى تحطيم التركيب البلوري ثلاثي البعد للطين و عزل طبقاته على شكل قشور نانوية ثنائية البعد, كما ان نمو البوليمر حول طبقات الطين المنعزلة عمل على زيادة الحجم الحبيبي الكلي للجسيمات على المقياس المجهري


Article
Comparison the Physical and Mechanical Properties of Composite Materials (Al /SiC and Al/ B4C) Produced by Powder Technology
مقارنة الخواص الفيزياوية والميكانيكية لمواد مركبة (المنيوم/ كاربيد السليكون، المنيوم/ كاربيد البورون) منتجة بطريقة تكنولوجيا المساحيق

Author: Khansaa Dawood Salman خنساء داود سلمان
Journal: Journal of Engineering مجلة الهندسة ISSN: 17264073 25203339 Year: 2017 Volume: 23 Issue: 10 Pages: 85-96
Publisher: Baghdad University جامعة بغداد

Loading...
Loading...
Abstract

In this investigation, metal matrix composites (MMCs) were manufactured by using powder technology. Aluminum 6061 is reinforced with two different ceramics particles (SiC and B4C) with different volume fractions as (3, 6, 9 and 12 wt. %). The most important applications of particulate reinforcement of aluminum matrix are: Pistons, Connecting rods etc. The specimens were prepared by using aluminum powder with 150 µm in particle size and SiC, B4C powder with 200 µm in particle size. The chosen powders were mixed by using planetary mixing setup at 250 rpm for 4hr.with zinc stearate as an activator material in steel ball milling. After mixing process the powders were compacted by hydraulic unidirectional press type (Leybold Harris No. 36110) at 250 Kg/cm2 according to (ASTM-D 618). Finally the green compacts were sintered at 500 ℃ for 3 hr. by using electrical furnace with argon atmosphere. There are many examinations and tests were done for the produced metal matrix composites (MMCS), (Al/ SiC and Al/B4C) such as examination of the microstructure, mechanical tests (hardness and compressive strength), physical tests (density test before and after sintering, also porosity test). The results of this investigation showed that improving the physical properties (theoretical density, experimental density, porosity) and mechanical properties (Rockwell hardness and compressive strength).

في هذا البحث تم تصنيع مادة مركبة بطريقة تكنولوجيا المساحيق. تمت تقوية الألمنيوم 6061 بنوعين مختلفين من الدقائق السيراميكية ( كاربيد السليكون ، كاربيد البورون) بنسب حجمية مختلفة 3، 6، 9، و12 % . من أهم تطبيقات التقوية بالدقائق لأرضية من الألمنيوم هي: المكابس، أذرع التوصيل . . الخ. تم تحضير العينات بأستخدام مسحوق الألمنيوم بحجم حبيبي 150 مايكرون ومساحيق كاربيد السليكون و كاربيد البورون بحجم حبيبي 200 مايكرون. تم خلط المساحيق المستخدمة باستخدام خلاط كوكبي بسرعة 250 دورة / دقيقة لمدة 4 ساعات مع مادة سترات الزنك كمادة منشطة مع كرات طحن من الفولاذ. بعد عملية الخلط تم تدميج المساحيق بمكبس هيدروليكي أحادي الأتجاه نوع (Leybold Harris No. 36110) بمقدار 250 كغم/ سم2 بموجب المواصفة (ASTM-D 618). أخيرآ تم تلبيد المدمجات الخضراء عند درجة حرارة 500مo لمدة 3 ساعات بأستخدام فرن كهربائي في جو من الآركون. أجريت العديد من الأختبارات والفحوصات للمواد المركبة المنتجة (ألمنيوم / كاربيد السليكون ، ألمنيوم/ كاربيد البورون ) مثل فحص البنية المجهرية ، أختبارات الصلادة ومقاومة الضغط، أختبارات الكثافة قبل وبعد التلبيد، كذلك أجري أختبار المسامية. أظهرت نتائج هذا البحث تحسن واضح في الخواص الفيزياوية (الكثافة النظرية ، الكثافة التجريبية، المسامية ) والخواص الميكانيكية (صلادة روكويل، مقاومة الأنضغاط).


Article
Effect of Temperature on Buckling of Composite Materials Column

Authors: Kadhim K. Resan --- Mohammed H. Ali --- Noor K. Faheed
Journal: AL-NAHRAIN JOURNAL FOR ENGINEERING SCIENCES مجلة النهرين للعلوم الهندسية ISSN: 25219154 / eISSN 25219162 Year: 2017 Volume: 20 Issue: 3 Pages: 511-519
Publisher: Al-Nahrain University جامعة النهرين

Loading...
Loading...
Abstract

A theoretical and experimental investigation pertaining to the buckling behavior of slender fiber reinforced polymer columns subjected to axial loading under varying temperatures (from room temperature to 50℃). Two groups of composite materials were used for manufacturing of test specimens, the first consist of perlon fiber as a reinforcement and acrylic resin as a bonding matrix, while the second consists of a combination of perlon and carbon fibers as reinforcement. The composite specimens were fabricated by vacuum molding technique and cut according to ASTM D-638 for conducting tensile test. The data from tensile test were used to calculate the effective slenderness ratio and defining the column as Euler buckling column. An experimental rig was designed, manufactured and calibrated to study the effect of thermal and buckling load subjected to columns.Numerical analyses pertaining the buckling behavior for both groups were conducted. The results show that the temperature has a considerable effect on properties of fiber reinforced polymer composites where the value of critical load and Young's Modules decrease with the increase of temperature for both groups. Perlon & Carbon reinforcement composites gave best mechanical properties, which make them the best candidate to improve the buckling resistance characteristics of composite materials.

يتناول البحث تحقيق نظري و تجريبي سلوك الانبعاج لأعمدة المصنوعه من الموادالبوليمريه المقوى بالألياف التي تخضع لحمل محوري في درجات حرارة متفاوتة (درجة حرارة الغرفة إلى 50 درجة مئوية). مجموعتان من المواد المركبة تم استخدامهما لإنتاج عينات الاختبار، الاولى تتكون من الياف البرلون كماده تقويه و(acrylic resin)كماده اساس رابطه بينما المجموعه الثانيه تتالف من الياف البرلون والكاربون كماده تقويه. تم تصنيع عينات الاختبار بواسطة تقنية ( (vacuum modelingوقطعت وفقا ل((ASTM D-638 لإجراء اختبار الشد. البيانات من اختبار الشد تم استخدامها لحساب نسبة النحول. في هذه الدراسة، تم تصميم جهازتجريبي خاص وتصنيعه ثم معايرته لغرض دراسة تأثير الحمل الحراري والانبعاج على الاعمده كما تم اجراءتحليل عددي يتناول سلوك الانبعاج لكلتا المجموعتين.أظهرت النتائج أن درجة الحرارة لها تأثير كبير على الخصائص مختلفة للمواد المركبه البوليمريه المقواه بالالياف حيث ان قيمة الحمل الحرج ومعامل المرونه تتناقص مع ارتفاع درجة الحرارة لكلا النوعين من المجموعات المركبة. المواد المركبه (مع الياف البرلون والكربون كماده تقويه) أظهرت خصائص ميكانيكيه افضلَ، التي تَجْعلُهم أفضل مرشّحِ لتَحسين خصائصِ مقاومةِ الانبعاج للموادِ المركّبه.


Article
دراسة بعض الخواص الفيزيائية و الميكانيكية لمادة متراكبة ذات اساس من الالمنيوم6063 مدعم بدقائق الزركونيا و المحضرة بتقانة ميتالورجيا المساحيق

Authors: نجيب سلمان عبطان --- رابحة صالح ياسين --- انمار ضيف مهدي
Journal: Journal of University of Babylon مجلة جامعة بابل ISSN: 19920652 23128135 Year: 2017 Volume: 25 Issue: 3 Pages: 932-941
Publisher: Babylon University جامعة بابل

Loading...
Loading...
Abstract

The aim of this work is studying some physical properties (density , porosity & water absorption) and some mechanical properties (micro hardness Vickers , compression strength & wear resistance) of aluminum 6063 matrix composite material that reinforced by (2.5,5,7.5&10) wt.% of ZrO2 particles. Powder metallurgy technique is used in samples preparing. Samples were compacted by using cold uniaxial pressing then followed sintering process at 600 oC under inert gas.Results were showed improving in (wear resistance , compression strength & micro hardness Vickers) and increasing in (density , porosity & water absorption). Increase micro hardness (44.5 – 101.13), compression strength (36.1998 – 46.7) N/mm2 and decrease wear rate (9.5*exp(-8) – 4.8*exp(-8)) g/cm at time 30 min. with (0 – 10)% ZrO2. While increase apparent density (1.388 – 3.15) g/cm3 , apparent porosity (0.96 – 4.61)% and water absorption (0.699 – 2.09)% at (0 – 10)% ZrO2.

يهدف البحث الى دراسة بعض الخواص الفيزيائية (الكثافة و المسامية و قابلية إمتصاص الماء) و بعض الخواص الميكانيكية (صلادة فيكرز المايكروية و مقاومة الإنضغاط القطرية و مقاومة البلى) لمادة متراكبة ذات اساس من الالمنيوم 6063 مدعمة بنسب وزنية مختلفة (2.5,5,7.5&10) wt.% من دقائق الزركونيا. وقد تم إتباع تقانة ميتالورجيا المساحيق في تحضير العينات حيث تم كبس العينات على البارد بطريقة الكبس احادي الإتجاه بضغط 5 طن تلى ذلك تلبيد العينات بدرجة حرارة 600 مo في جو خامل.وقد اظهرت النتائج ان تدعيم الالمنيوم 6063 بدقائق الزركونيا تحسن من مقاومة البلى و مقاومة الإنضغاط و صلادة فيكرز المايكروية وكذلك زيادة في قيم الكثافة و المسامية و قابلية إمتصاص الماء . إذ تزداد الصلادة من (101.13 – 44.5) و مقاومة الإنضغاط القطرية من (46.7 – 36.1998) N/mm2و يقل معدل البلى من (4.8*exp(-8) – 9.5*exp(-8)) غم/سم عند زمن 30 دقيقة ومحتوى (0 – 10)% من الزركونيا. بينما تزداد الكثافة الظاهرية (3.15 – 1.388) غم/سم3 و المسامية الظاهرية (4.61 – 0.96)% و قابلية إمتصاص الماء (2.09 – 0.699)% عند محتوى (10 – 0)% من الزركونيا.

Listing 1 - 10 of 12 << page
of 2
>>
Sort by
Narrow your search

Resource type

article (12)


Language

English (11)

Arabic (1)


Year
From To Submit

2017 (12)