Article
The effect of TiO2 addition on the thermal conductivity of Polymethylmetha acrylate, Polycarbonate and Polystyrene Polymers
تأثير اضافة اوكسيد التيتانيوم على التوصيلية الحرارية لبوليمرات البولي مثيل ميثا اكريليت, البولي كاربونيت و البولي ستايرين

Loading...
Loading...
Abstract

Thermal conductivity measurement was done for specimens of Polystyrene/ titanium dioxide, Polycarbonate/ titanium dioxide and Polymethylmetha acrylate/ titanium dioxide composites for weight ratio of 1.9/ 0.1 and 1.8/ 0.2 wt% for different thickness of the samples. The experimental results show that the thermal conductivity is increased with the increasing of thickness of layers and with the weight ratio of TiO2.

تم في هذا البحث دراسة التوصيلية الحراراية لعينات من متراكبات البولي ستايرين / ثاني اوكسيد التيتانيوم, البولي كاربونيت / ثاني اوكسيد التيتانيوم و البولي مثيل ميثا اكريليت / ثاني اوكسيد التيتانيوم وبنسب وزنية 0.1/1.9و 0.2/1.8من ثاني اوكسيد التيتانيوم .تشير النتائج الى ان التوصيلية الحرارية تزداد بزيادة كل من سمك طبقة المتراكب ونسبة تركيز ثاني اوكسيد التيتانيوم .


Article
Structural and Optical Properties of Annealed TiO2 Powder Synthesized by Hydrothermal Method
الخصائص الهيكلية والبصرية من مسحوق ثاني أكسيد التيتانيوم النانوي توليفها بواسطة طريقة الحرارية المائية

Authors: Sariya D. Al-Algawi ساريه العلكاوي --- Rashed T. Rasheed راشد رشيد --- Zeena R. Rhoomi زينة رباح رحومي
Journal: Iraqi Journal of Science المجلة العراقية للعلوم ISSN: 00672904/23121637 Year: 2017 Volume: 58 Issue: 3C Pages: 1683-1693
Publisher: Baghdad University جامعة بغداد

Loading...
Loading...
Abstract

Titanium dioxide (TiO2) Nano powder has been synthesized by hydrothermal method. The reaction took place between titanium tetrachloride (TiCI4) and mixture solution consisted of deionized water and ethanol, in the ratio (3:7) respectively. Structure and surface morphology of TiO2 Nano powder at different annealing temperatures in the range 200-800°C for 120 min were characterized by X-ray diffraction (XRD), Atomic Force Microscope (AFM), Scanning Electron Microscopy (SEM), FT-IR and UV/visible spectroscopy measurements. The results show that with an increase in annealing temperature, the value of the intensity of (110) peak for rutile phase increases while the value of the full-width at half maximum (FWHM) decreases, and the band gap decreases with increasing temperature.

حضر اوكسيد التيتانيوم بتقنية الحراره المائيه في الأوتكليف، حصل التفاعل بين رباعي كلوريد التيتانيوم ومزيج متكون من ماء لاايوني وايثانول بنسبة (37:) بالتتابع. تركيب وطبغرافية السطح لاوكسيد التيتانيوم النانوي الملدن بدرجات حرارية مختلفة (200-800) ͦ م لمدة 120 دقيقة تم تشخيصها بواسطة قياسات حيود الاشعة السينية (XRD)، مجهر القوة الذرية (AFM)، المجهر الألكتروني الماسح (SEM) ومطيافية الأشعة تحت الحمراء (FT-IR) والأشعة فوق البنفسجية/المرئية (UV/Visible). اظهرت النتائج ان شدة القمة (110) لطور روتايل تزداد بزيادة درجة حرارة التلدين بينما العرض عند منتصف الارتفاع (FWHM) يقل وان فجوة الطاقة تقل مع زيادة درجة حرارة التلدين.


Article
Photocatalytic Degradation of Cobalamin by Metalized TiO2

Authors: Ahmed F. Halbus --- Falah H. Hussein
Journal: Journal of University of Babylon مجلة جامعة بابل ISSN: 19920652 23128135 Year: 2012 Volume: 22 Issue: 1 Pages: 445-453
Publisher: Babylon University جامعة بابل

Loading...
Loading...
Abstract

The purpose of this study was to investigate experimentally the degradation of cobalamin by suspensions of platinum and other metals supported on Hombikat UV100 . The effect of temperature on the efficiency of photodegradation of cobalamin was studied in the range 278-298K using UVA source of irradiation. The activation energy was calculated according to Arrhenius plot, and was found equal to 22 ±1 kJ.mol-1 for TiO2. The results showed that pH of reactants was changed at the end of reaction towards 7 independent on the initial pH .The results of the total organic carbon (TOC) analysis indicate that the rate of degradation of dye was faster than the total mineralization. Decolorization and mineralization of cobalamin in the absence of light and/or catalyst were performed to demonstrate that the presence of light and catalyst is essential for the degradation of this cobalamin. The results show that the activity of different types of metals used in this study was in the following the sequence:Pt/TiO2 > Pd/TiO2 > Au/TiO2


Article
Solar Photocatalytic Degradation of Diuron in Aqueous Solution by TiO2
تحلل الدوران في محلول مائي بالتحفيز الضوئي بواسطة ثنائي أوكسيد التيتانيوم باستخدام الطاقة الشمسية

Authors: Yasmen A. Mustafa ياسمين عبد العزيز مصطفى --- Hussain Ali Al-Jobouri حسين علي احمد
Journal: Journal of Engineering مجلة الهندسة ISSN: 17264073 25203339 Year: 2014 Volume: 20 Issue: 11 Pages: 80-90
Publisher: Baghdad University جامعة بغداد

Loading...
Loading...
Abstract

The solar photocatalytic degradation of diuron, which is one of the herbicides, has been studied by a solar pilot plant in heterogeneous solar photocatalysis with titanium dioxide. The pilot plant was made up of compound parabolic collectors specially designed for solar photocatalytic applications. The influence of different variables such as, H2O2 initial concentration, TiO2 initial concentration, and diuron initial concentration with their relationship to the degradation efficiency were studied. Hydrogen peroxide (H2O2) found to increase the rate of diuron degradation. The best removal efficiency of heterogeneous solar photocatalytic TiO2 system was found to be 46.65 % and for heterogeneous solar photocatalytic TiO2/ H2O2 system was found to be 80.65 %. Based on these results, the solar photocatalytic degradation by TiO2/ H2O2 system could be a useful technology for the treatment of effluents containing diuron.

تمت دراسة التحلل بالتحفيز الضوئي للمبيد (ديورون -(diuron وهو أحد أنواع مبيدات الادغال/ الأعشاب بواسطة منظومة تعمل بنظام الاكسدة المتقدمة الغير متجانس (التحفيز الضوئي بثنائي أوكسيد التيتانيوم) باستخدام الطاقة الشمسية. تتكون المنظومة الريادية من مجمعات القطع المكافئ المركبة (compound parabolic collectors) مصممة خصيصا لتطبيقات التحفيز الضوئي بالطاقة الشمسية. درست تأثير المتغيرات المختلفة مثل التركيز الأولي لبيروكسيد الهيدروجين والتركيز الاولي لثنائي أوكسيد التيتانيوم والتركيز الاولي للمبيد وتأثيرها على كفاءة الازالة. وجد ان بيروكسيد الهيدروجين يزيد من معدل تحلل المبيد (ديورون). كانت أفضل كفاءة إزالة التحفيز الضوئي باستخدام نظام التحلل بواسطة ثنائي أوكسيد التيتانيوم لوحده تساوي 46.65 % وباستخدام نظام التحلل بواسطة ثنائي أوكسيد التيتانيوم مع بيروكسيد الهيدروجين كفاءة الازالة تساوي 80.65 %. بناء على هذه النتائج فان التحلل بالتحفيز الضوئي بواسطة الطاقة الشمسية باستخدام نظام ثنائي أوكسيد التيتانيوم مع بيروكسيد الهيدروجين يمكن ان تكون تكنولوجيا مفيدة لمعالجة المطروحات الحاوية على مبيد الديورون.


Article
Medium Energy Ion Scattering Spectrometry of Helium Ions Scattered from Rutile Titanium Dioxide Surfaces

Author: Zaid H. Mhsin, Nawal K. Gafil
Journal: Iraqi Journal of Applied Physics المجلة العراقية للفيزياء التطبيقية ISSN: 18132065 23091673 Year: 2018 Volume: 14 Issue: 3 Pages: 29-33
Publisher: iraqi society for alternative and renewable energy sources and techniques الجمعية العراقية لمصادر وتقنيات الطاقة البديلة والمستجدة

Loading...
Loading...
Abstract

The charge state of medium energy He ions scattered from solid surfaces depends on emerging energy and angle as well as the surface materials. We measured He+ fractions for 54-140keV He+ ions incident on rutile TiO2(110) and scattered from the top-layer Ti atoms at the [110]- and [001]-azimuth. The He+ fractions measured at both azimuths were decreased with increasing emerging angle (scaled from surface normal) and saturated at ~75 and ~85° at the [001]- and [110]-azimuth, respectively. The He+ fractions for the [110]-azimuth denoted by η110 were considerably larger by 10-20% than those for the [001]-azimuth (η) at emerging angles below ~75° (non-equilibrated). The equilibrium He+ fraction is close to the semi-empirical data given by Marion-Young. It was also found that the η110 values measured at emerging angle of ~80° were larger more than 20% compared with the η values in the emerging energy range from 50 to 130keV. Such a strong dependence on crystallographic orientation of scattering plane is simply explained by the atomic arrangements at the crystalline azimuths.


Article
Effect of Gas Mixing Ratio on Energy Band Gap of Mixed-Phase Titanium Dioxide Nanostructures Prepared by Reactive Magnetron Sputtering Technique

Authors: Esraa A. Al-Oubidy --- Firas J. Al-Maliki
Journal: Iraqi Journal of Applied Physics المجلة العراقية للفيزياء التطبيقية ISSN: 18132065 23091673 Year: 2018 Volume: 14 Issue: 4 Pages: 19-23
Publisher: iraqi society for alternative and renewable energy sources and techniques الجمعية العراقية لمصادر وتقنيات الطاقة البديلة والمستجدة

Loading...
Loading...
Abstract

In this work, a homemade dc closed-field unbalanced reactive magnetron sputtering system was used to prepare high-quality and highly pure titanium dioxide nanostructures. The operation parameters of the magnetron sputtering system were optimized to prepare TiO2 nanostructures as thin films on glass substrates. These films were characterized by x-ray diffraction, scanning electron microscopy, atomic force microscopy and Fourier-transform infrared spectroscopy. Both anatase and rutile phases were identified. From the UV-visible spectroscopy, the indirect energy band gap was determined to be 3.30-3.38 eV. The mixing ratio of argon and oxygen (Ar:O2) gases was found very important to control the structural and optical characteristics of the prepared nanostructures.


Article
The Growth Characteristics of RF-Magnetron Sputtered Nanocrystalline TiO2 Thin Films

Authors: Azhar K. Sadkhan --- Suaad A. Mohammed --- Mohammed K. Khalaf
Journal: Engineering and Technology Journal مجلة الهندسة والتكنولوجيا ISSN: 16816900 24120758 Year: 2018 Volume: 36 Issue: 2 Part (B) Engineering Pages: 128-130
Publisher: University of Technology الجامعة التكنولوجية

Loading...
Loading...
Abstract

In this paper, RF Magnetron sputtered TiO2 thin films deposited onglass slices at various powers (75,100,125 and 150) Watt for (1.5) hour anddifferent thickness (62.5-88-118 and 132.6) nm, the TiO2 thin films annealed with400°C for 2 hour and the morphology and structure of these films are describedby X-ray diffraction XRD and atomic force microscopy AFM to show the phasestructure. X-ray diffraction investigation uncovered that the crystalline size of theTiO2 thin films displays an expanding pattern with increasing the sputteringpower. The preferred orientation of (101) was watched for the films depositedwith sputtering power of (75,100,125 and 150) Watt


Article
Production of TiO2 Nanoparticles in Different Phases and Shapes by using PLA and Hydrothermal Method

Authors: Abbas K. Jarallah --- Raad S. Sabry --- Wisam J. Aziz
Journal: Al-Mustansiriyah Journal of Science مجلة علوم المستنصرية ISSN: 1814635X Year: 2018 Volume: 29 Issue: 2 Pages: 175-178
Publisher: Al-Mustansyriah University الجامعة المستنصرية

Loading...
Loading...
Abstract

Titanium dioxide was prepared using pulsed laser ablation (PLA) and hydrothermal method. Scanning electron microscopy images showed that the product from hydrothermal method had a nanotube shape, whereas those from PLA in liquid were nanoparticles. The optical properties in the absorption curve of product from the hydrothermal method were slightly greater than those from the PLA method, and the energy gaps were 3.39 and 3.26 eV for the hydrothermal method and PLA, respectively. XRD results showed that the TiO2 prepared through PLA showed one phase (rutile), whereas those prepared through hydrothermal method showed two phases (anatase and rutile). Moreover, the product from hydrothermal method had smaller particle size smaller than that from PLA. Furthermore, the product yield and the required reaction time of the hydrothermal method were higher than those of PLA.

في هذا البحث تم تحضير مادة اوكسيد التيتانيوم بطريقة القشط بالليزر النبظي وطريقة الهايدروثيرمال. اظهرت صور المجهر الالكتروني الماسح بان التشكيل المتكون على السطح بطريقة الهايدروثيرمال هي اشكال انابيب دقيقه ولكن الاشكال الظاهرة بطريقة القشط بالليزر هي اشكال كرويه.الخصائص البصريه اظهرت من خلال منحني الامتصاص بان الامتصاصيه بطريقة الهايدروثيرمال هي اكبر بقليل من الامتصاص الناتج بطريقة القشط بالليزر وان فجوة الطاقه كانت (3.26 eV -3.39 eV ) للنماذج المحضره بطريقة الهايدروثيرمال والليزر على التوالي. نتائج حيود الاشعه السينيه اظهرت بان ثنائي اوكسيد التيتانيوم الناتج بطريقة الليزر كان بطور واحد هو الروتايل بينما كان بطورين هما ( الروتايل والاناتاس ) بطريقة الهايدروثيرمال اضافة الى ذلك فان حجم الجسيمات الناتجه بواسطة الهايدروثيرمال كان اصغر من حجم الجسيمات الناتجه بطريقة الليزر وكذلك الزمن المطلوب لاتمام التفاعل بطريقة الهايدروثيرمال يكون اطول من الزمن اللازم بطريقة الليزر.


Article
KINETIC STUDY OF PHOTODEGRADATION OF Azo DYES WITH TiO2 UNDER VISIBLE LIGHT

Authors: Hassan A. Habeeb --- Abbas A. A. Kadhum
Journal: Al-Nahrain Journal of Science مجلة النهرين للعلوم ISSN: (print)26635453,(online)26635461 Year: 2010 Volume: 13 Issue: 3 Pages: 41-50
Publisher: Al-Nahrain University جامعة النهرين

Loading...
Loading...
Abstract

In this work, two mono azo dyes : 4-(2- benzoic acid azo )-m-amino phenol (BAMAP), and4-(2-benzoic acid azo)-P-amino phenol (BAPAP)have been synthesized and identified by FT-IRspectroscopy. UV-Visible absorption spectra were recorded and some physical and chemicalproperties have been listed.The photodegradation of dyes was investigated by using the light of tungsten lamp in presenceand absence of titanium dioxide (anatase). It has been found that the increasing of TiO2 masscaused an increasing in photodegradation of two dyes until the optimum mass (2gm/l) was reached.Also, the results indicate, that the basic media give more photodegradation rate than acidic medium,moreover ,the effect of temperatures in the range (298 323K) on degraded dye was studied ,and theactivation energy of photodegradation processes was calculated from Arrhenius plot which equal35.82KJ.mol-1for BAMAP and 32.11KJ.mol-1for BAPAP.The results showed the photoreaction is1st order ,with decomposition constant equal 2.362x10-4min-1for BAMAP and 2.826x10-4 min-1forBAPAP at 298k and neutral medium.Generally, it has been found that the rate of photodegradation of BAPAP is more than BAMAP,and the decolonization rate of the two dyes was higher in presence of TiO2 suspension.

يتضمن البحث تحضير صبغتي ازو أحادية وهما(PAPAP) -2 حامض البنزويك ازو ) بارا امينو فينول )-42- حامض البنزويك ازو ) ميتا امينو فينول )- و 4تم تشخيص الأصباغ المحضرة بوساطة . (PAMAP)مطيافية الأشعة تحت الحمراء. و سجلت كذلك أطيافالأشعة المرئية وفوق البنفسجية وتم دراسة بعض الخواصالفيزيائية والكيميائية .وتضمن البحث كذلك دراسة التحطم الضوئي للأصباغالمحضرة بوساطة استخدام ضوء من مصباح مرئي بوجودوغياب عالق ثاني اوكسيد التيتانيوم (الانتيز) .وجد إنأدت إلى زيادة سرعة التحطم الضوئي TiO زيادة تركيز 2TiO لكلا الصبغتين لحين الوصول إلى التركيز الأمثل ل 2وهو 2غم/لتر . ودلت النتائج أيضا بان المحيط القاعدي قدحفز من سرعة التحطم الضوئي أكثر بالمقارنة مع المحيطألحامضي .درس تأثير درجة الحرارة ضمن المدى - 323298 كلفن حيث وجد آن درجات الحرارة العالية أدت إلىزيادة سرعة تحطم الصبغتين ووجد إن طاقة التنشيط كانتو PAMAP 35.82 كيلو جول/مول للصبغةللصبغة.دلت PAPAP 32.11 كيلو جول/مول للصبغةالنتائج بان التفاعل الضوئي المحفز تبع حر كيات منالمرتبة الأولى ووجد أن ثابت سرعة التفككو PAMAP 2.362 للصبغة x 10-4 min-1. PAPAP 2.826 للصبغة x 10-4 min-1و بصورة عامة وجد بان سرعة التحطم الضوئي، BAMAP كانت أعلى من الصبغة BAPAP للصبغةكذلك فان سرعة إزالة اللون لكلا الصبغتين كانت أعلى. TiO بوجود عالق 2


Article
"Deposition of Colloidal Titanium Oxide Nanoparticles using Pulsed Nd: YAG Laser Ablation in Liquid to Increase the Efficiency of the Si Solar Cell"

Authors: Amenah Ali Salman --- Hiba S. Tarik --- Khaled Z. Yahea
Journal: Al-Nahrain Journal of Science مجلة النهرين للعلوم ISSN: (print)26635453,(online)26635461 Year: 2014 Volume: 17 Issue: 1 Pages: 103-108
Publisher: Al-Nahrain University جامعة النهرين

Loading...
Loading...
Abstract

This work reports the attempts to carry out pulsed laser ablation in liquid (PLAL) for synthesizing colloidal Titanium dioxide nanoparticles (NPs). TiO2 NPs was synthesized by 7ns Nd:YAG laser ablation of high purity titanium target (99.99 %) immersed in water ,and deposited the film on silicon solar cell to increase the efficiency of the Si solar cell . The surface morphology of the deposits materials have been studied by using atomic force microscopes (AFM). Atomic Force Microscopy(AFM) analysis showed that the average grain size of TiO2NPsinwater were 150 nm and rms roughness values are (2.27 nm) for TiO2 thin film. The photovoltaic characteristics before and after deposited Titanium dioxide nanoparticles (NPs) included short circuit current (Jsc),open circuit voltage (Voc), where the maximum (Jsc), (Voc)and fill factor (FF) obtained at AM1after deposited were 40.2 (mA cm-2) , 630(mV) and(0.7) respectively. After deposited Titanium dioxide nanoparticles (NPs)increase the efficiency of the Si solar cell13.8 % instead of 10.3% conversion efficiency before the deposited.

يهدف ھذا البحث الى تحضيرمحلول للجسيمات النانوية لاوكسيد التيتانيوم باستخدام طريقة الاستئصال بالليزر النبضي تم تحضير الجسيمات النانوية لاوكسيد التيتانيوم بزمن 7 نانوثانية بواسطة الليزر نوع نيديميوم ياك لهدف من التيتانيوم عالي النقاوة (99.99 %) مغطس بالماء, ثم ترسيب غشاء اوكسيد التيتانيوم النانوي على سطح خلية شمسية سليكونية وذلك لزيادة كفاءتها. تم دراسة طبيعة السطح لجسيمات الاوكسيد النانوية باستخدام مجهر القوى الذرية حيث بينت تحاليل مجهر القوى الذريةAFM )) ان معدل الحجم الحبيبي لجسيمات الاوكسيد المستئصلة بالماء هي 150 نانو متر وبلغت قيمة خشونة السطح لغشاء اوكسيد التيتانيوم 2.27 نانو متر. درست الخواص الفولطائية للخلية قبل وبعد ترسيب جسيمات اوكسيدالتيتانيوم النانوية المتمثلة بتيار دائرة القصر (Jsc), وفولتية الدائرة المفتوحة (Voc), بالاضافة لعامل الملئ(FF) لحالة AM1 حيث بلغت قيمتهم بعد الترسيب 40.2 (mA cm-2), 630(mV),و 0.7 على التوالي. لقد ازدادت قيمة كفاءة الخلية الشمسية الى 13.8 % بدلا" من 10.3 % بعد ترسيب غشاء اوكسيد التيتانيوم النانوي.

Listing 1 - 10 of 27 << page
of 3
>>
Sort by
Narrow your search

Resource type

article (27)


Language

English (25)

Arabic (2)


Year
From To Submit

2019 (3)

2018 (9)

2017 (2)

2016 (1)

2015 (1)

More...